Natural minerals mixture for enhancing concrete compressive strength
The construction material quality is required to be improved in order to enhancing structure stability, optimizing construction cost and quality. The kaolin and bentonite have been mixed in equal quantity and treated by heat for 1 hour under 600 ºC, 800 ºC and 1000 ºC to create new minerals under hi...