Effect of LF Soft Bubbling Time on Inclusions in Tire Cord Steel LX82 A
For the control of cord steel inclusion, long time soft bubbling treatment is usually chosen to improve the cleanliness of molten steel, but it will lead to the increased erosion of magnesia-carbon bricks. Through the industrial production test, the effects of soft blowing time after LF refining on...
Saved in:
| Main Author: | Zhao Haoqian, Zhang Yuming, Ma Bo, Gong Yanjie, Meng Yaoqing |
|---|---|
| Format: | Article |
| Language: | zho |
| Published: |
Editorial Office of Special Steel
2024-11-01
|
| Series: | Teshugang |
| Subjects: | |
| Online Access: | http://www.specialsteeljournal.com/fileup/1003-8620/PDF/2024-00099.pdf |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Thermodynamic modeling of deoxidation products and inclusion chemistry in Mn/Si killed tire-cord steel
by: Prasad A.D., et al.
Published: (2012-01-01) -
Treatment of LF slag to prevent powdering during cooling
by: Ghorai S., et al.
Published: (2017-01-01) -
Predicting the Wear Amount of Tire Tread Using 1D−CNN
by: Hyunjae Park, et al.
Published: (2024-10-01) -
Analysis of Tire-Road Interaction: A Literature Review
by: Haniyeh Fathi, et al.
Published: (2024-11-01) -
Basic framework and key technologies of parallel tires
by: Xiangwen ZHANG, et al.
Published: (2022-09-01)