Failure analysis of dissimilar single-lap joints

Single-lap joints made of aluminium and carbon fibre adherends of different thickness are tested to understand better the behaviour of such dissimilar joints. The overlap length and the thickness of the adhesive are kept constant. Local deformation fields are onitored by using the digital image corr...

Full description

Saved in:
Bibliographic Details
Main Authors: F.A. Stuparu, D.A. Apostol, D.M. Constantinescu, M. Sandu, S. Sorohan
Format: Article
Language:English
Published: Gruppo Italiano Frattura 2016-03-01
Series:Fracture and Structural Integrity
Subjects:
Online Access:http://www.gruppofrattura.it/pdf/rivista/numero36/numero_36_art_8.pdf
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:Single-lap joints made of aluminium and carbon fibre adherends of different thickness are tested to understand better the behaviour of such dissimilar joints. The overlap length and the thickness of the adhesive are kept constant. Local deformation fields are onitored by using the digital image correlation method. Peeling and shearing strains are investigated, emphasizing that peeling is important in the region where failure is initiated, towards an extremity of the overlap region. The use of only carbon fibre adherends is not recommended for a smaller thickness as an additional interface failure is produced and compromises the integrity of the lap joint. However, a dissimilar joint (aluminium-carbon) with smaller thickness adherends succeeds to maintain the stiffness of the assembly, but its strength is diminished. The obtained results are suggesting that a complete monitoring of the failure processes in the overlap region can be fully understood only if local deformation measurements are possible.