THERMAL DEFORMATION CONDITIONS FOR THE FORMATION OF HOLLOW CYLINDRICAL CAST IRON CASTING IN THE METAL WATER-COOLED FORM
An experimental and calculated thermal analysis of the bronze billets continuous casting plant is developed. Allowable thermal conditions for rolling-out are calculated.
Saved in:
| Main Authors: | E. I. Marukovich, V. F. Bevza, V. A. Popkovsky, V. P. Grusha |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Belarusian National Technical University
2013-09-01
|
| Series: | Литьë и металлургия |
| Online Access: | https://lim.bntu.by/jour/article/view/159 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
PRINCIPALLY NEW EFFECTIVE CASTING PROCESS OF THE HOLLOW CYLINDRICAL SLUGS OF CAST IRON BY METHOD OF DIRECTIONAL SOLIDIFICATION
by: E. I. Marukovich, et al.
Published: (2010-08-01) -
FORMING OF HOLLOW SLUGS OF CAST IRON WITH GLOBULAR GRAPHITE IN CONDITIONS OF WALL CRYSTALLIZATIO
by: V. F. Bevza, et al.
Published: (2009-08-01) -
LONGITUDINAL DIFFERENT-WALL OF HOLLOW CASTINGS AT FORMING OF INTERNAL SURFACE OUT OF MELT WITHOUT APPLICATION OF ROD
by: E. I. Marukovich, et al.
Published: (2006-05-01) -
THEORETICAL AND TECHNOLOGICAL BASIS OF CASTING OF HOLLOW BILLETS BY THE METHOD OF DIRECTIONAL SOLIDIFICATION
by: E. I. Marukovich, et al.
Published: (2011-05-01) -
HARDENING OF CASTINGS AT FREE FORMING OF INTERNAL SURFACE
by: E. I. Marukovich, et al.
Published: (2005-08-01)