High Temperature Isothermal Oxidation at 950°C of Ni-based Fe-40Ni-24Cr Alloy

The effect of different heat treatment temperatures on the isothermal oxidation of Ni-based Fe-40Ni-24Cr alloy was studied. The alloy underwent a heat treatment process at 1000°C and 1200°C for 3 hours of soaking time, followed by water quenching. These samples are labeled as N10 and N12. The heat-t...