Failure analysis of dissimilar single-lap joints

Single-lap joints made of aluminium and carbon fibre adherends of different thickness are tested to understand better the behaviour of such dissimilar joints. The overlap length and the thickness of the adhesive are kept constant. Local deformation fields are monitored by using the digital image cor...