Formation of a Boron‐Oxide Termination for the (100) Diamond Surface
Abstract A boron‐oxide termination of the diamond (100) surface has been formed by depositing molecular boron oxide B2O3 onto the hydrogen‐terminated (100) diamond surface under ultrahigh vacuum conditions and annealing to 950 °C. The resulting termination is highly oriented and chemically homogeneo...