Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge

Lithium-ion batteries risk failing when subjected to different abuse tests, resulting in gas and flames. In this study, 5 Ah nickel manganese cobalt oxide (NMC) pouch cells were subjected to external heating; overcharge at rates of 2.5, 5 and 10 A; and nail penetration. Tests were conducted in air a...

Full description

Saved in:
Bibliographic Details
Main Authors: Gemma E. Howard, Katie C. Abbott, Jonathan E. H. Buston, Jason Gill, Steven L. Goddard, Daniel Howard
Format: Article
Language:English
Published: MDPI AG 2025-05-01
Series:Batteries
Subjects:
Online Access:https://www.mdpi.com/2313-0105/11/5/197
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1849327705812631552
author Gemma E. Howard
Katie C. Abbott
Jonathan E. H. Buston
Jason Gill
Steven L. Goddard
Daniel Howard
author_facet Gemma E. Howard
Katie C. Abbott
Jonathan E. H. Buston
Jason Gill
Steven L. Goddard
Daniel Howard
author_sort Gemma E. Howard
collection DOAJ
description Lithium-ion batteries risk failing when subjected to different abuse tests, resulting in gas and flames. In this study, 5 Ah nickel manganese cobalt oxide (NMC) pouch cells were subjected to external heating; overcharge at rates of 2.5, 5 and 10 A; and nail penetration. Tests were conducted in air and N<sub>2</sub> atmospheres. Additional external heat tests were performed on cells at 5, 25, 50, and 75% SoC and on two, three, and four cell blocks. Gas volumes were calculated, and the gas composition was given for H<sub>2</sub>, CO, CO<sub>2</sub>, C<sub>2</sub>H<sub>4</sub>, C<sub>2</sub>H<sub>6</sub>, CH<sub>4</sub>, C<sub>3</sub>H<sub>6</sub>, and C<sub>3</sub>H<sub>8</sub>. For tests under an air atmosphere at 100% SoC, the volume of gas varied between abuse methods: 3.9 L (external heat), 6.4 L (overcharge), and 8.9 L (nail penetration). The gas composition was found to predominantly contain H<sub>2</sub>, CO<sub>2</sub>, and CO for all abuse methods; however, higher concentrations of H<sub>2</sub> and CO were present in tests performed under N<sub>2</sub>. External heat tests at different SoCs showed that the gas volume decreased with SoC. Overall, the type of abuse method can have a large effect on the gas volume and composition produced by cell failure.
format Article
id doaj-art-37b99b5bd88a4b478422dbb4d3ee2ae1
institution Kabale University
issn 2313-0105
language English
publishDate 2025-05-01
publisher MDPI AG
record_format Article
series Batteries
spelling doaj-art-37b99b5bd88a4b478422dbb4d3ee2ae12025-08-20T03:47:48ZengMDPI AGBatteries2313-01052025-05-0111519710.3390/batteries11050197Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of ChargeGemma E. Howard0Katie C. Abbott1Jonathan E. H. Buston2Jason Gill3Steven L. Goddard4Daniel Howard5HSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UKHSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UKHSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UKHSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UKHSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UKHSE Science and Research Centre, Harpur Hill, Buxton SK17 9JN, UKLithium-ion batteries risk failing when subjected to different abuse tests, resulting in gas and flames. In this study, 5 Ah nickel manganese cobalt oxide (NMC) pouch cells were subjected to external heating; overcharge at rates of 2.5, 5 and 10 A; and nail penetration. Tests were conducted in air and N<sub>2</sub> atmospheres. Additional external heat tests were performed on cells at 5, 25, 50, and 75% SoC and on two, three, and four cell blocks. Gas volumes were calculated, and the gas composition was given for H<sub>2</sub>, CO, CO<sub>2</sub>, C<sub>2</sub>H<sub>4</sub>, C<sub>2</sub>H<sub>6</sub>, CH<sub>4</sub>, C<sub>3</sub>H<sub>6</sub>, and C<sub>3</sub>H<sub>8</sub>. For tests under an air atmosphere at 100% SoC, the volume of gas varied between abuse methods: 3.9 L (external heat), 6.4 L (overcharge), and 8.9 L (nail penetration). The gas composition was found to predominantly contain H<sub>2</sub>, CO<sub>2</sub>, and CO for all abuse methods; however, higher concentrations of H<sub>2</sub> and CO were present in tests performed under N<sub>2</sub>. External heat tests at different SoCs showed that the gas volume decreased with SoC. Overall, the type of abuse method can have a large effect on the gas volume and composition produced by cell failure.https://www.mdpi.com/2313-0105/11/5/197Li-ionpouch cellnickel manganese cobalt oxideexternal heatoverchargenail penetration
spellingShingle Gemma E. Howard
Katie C. Abbott
Jonathan E. H. Buston
Jason Gill
Steven L. Goddard
Daniel Howard
Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
Batteries
Li-ion
pouch cell
nickel manganese cobalt oxide
external heat
overcharge
nail penetration
title Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
title_full Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
title_fullStr Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
title_full_unstemmed Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
title_short Comprehensive Study of the Gas Volume and Composition Generated by 5 Ah Nickel Manganese Cobalt Oxide (NMC) Li-Ion Pouch Cells Through Different Failure Mechanisms at Varying States of Charge
title_sort comprehensive study of the gas volume and composition generated by 5 ah nickel manganese cobalt oxide nmc li ion pouch cells through different failure mechanisms at varying states of charge
topic Li-ion
pouch cell
nickel manganese cobalt oxide
external heat
overcharge
nail penetration
url https://www.mdpi.com/2313-0105/11/5/197
work_keys_str_mv AT gemmaehoward comprehensivestudyofthegasvolumeandcompositiongeneratedby5ahnickelmanganesecobaltoxidenmcliionpouchcellsthroughdifferentfailuremechanismsatvaryingstatesofcharge
AT katiecabbott comprehensivestudyofthegasvolumeandcompositiongeneratedby5ahnickelmanganesecobaltoxidenmcliionpouchcellsthroughdifferentfailuremechanismsatvaryingstatesofcharge
AT jonathanehbuston comprehensivestudyofthegasvolumeandcompositiongeneratedby5ahnickelmanganesecobaltoxidenmcliionpouchcellsthroughdifferentfailuremechanismsatvaryingstatesofcharge
AT jasongill comprehensivestudyofthegasvolumeandcompositiongeneratedby5ahnickelmanganesecobaltoxidenmcliionpouchcellsthroughdifferentfailuremechanismsatvaryingstatesofcharge
AT stevenlgoddard comprehensivestudyofthegasvolumeandcompositiongeneratedby5ahnickelmanganesecobaltoxidenmcliionpouchcellsthroughdifferentfailuremechanismsatvaryingstatesofcharge
AT danielhoward comprehensivestudyofthegasvolumeandcompositiongeneratedby5ahnickelmanganesecobaltoxidenmcliionpouchcellsthroughdifferentfailuremechanismsatvaryingstatesofcharge