Development of High Temperature Oxidation Technology for SiC and Analysis on the Characteristics of its Interface

It used n-type 4° off-axis 4H-SiC (0001) substrates to form SiO2 layers by thermal oxidation in the condition of 1 200 ℃, 1 250 ℃, 1 300 ℃as well as 1 350 ℃, and analyzed the SiO2/SiC interface via the C-V and I-V characteristics of MOS capacitor structure. The results show that the interface state...