Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10Mg

This study investigates the impact of low-temperature stress-relieving treatment on the fatigue life of AlSi10Mg components produced by Laser Powder Bed Fusion (L-PBF). The research focuses on a bicycle crank arm, comparing its performance in as-built and heat-treated conditions. The heat treatment...

Full description

Saved in:
Bibliographic Details
Main Authors: Malcolm António, Rui Fernandes, Joel de Jesus, Luís Borrego, Ricardo Branco, José da Costa, José Ferreira
Format: Article
Language:English
Published: MDPI AG 2024-12-01
Series:Applied Sciences
Subjects:
Online Access:https://www.mdpi.com/2076-3417/15/1/112
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1841549473707196416
author Malcolm António
Rui Fernandes
Joel de Jesus
Luís Borrego
Ricardo Branco
José da Costa
José Ferreira
author_facet Malcolm António
Rui Fernandes
Joel de Jesus
Luís Borrego
Ricardo Branco
José da Costa
José Ferreira
author_sort Malcolm António
collection DOAJ
description This study investigates the impact of low-temperature stress-relieving treatment on the fatigue life of AlSi10Mg components produced by Laser Powder Bed Fusion (L-PBF). The research focuses on a bicycle crank arm, comparing its performance in as-built and heat-treated conditions. The heat treatment involved stress-relieving at 250 °C for 2 h, followed by water quenching. The study found that the as-built condition exhibited a supersaturated Si cellular-dendritic microstructure, while the heat-treated condition showed coarsening of β-Mg<sub>2</sub>Si phases and Si precipitates. This morphological change led to a decrease in hardness and an increase in ductility. Fatigue tests demonstrated that the heat-treated crank arms achieved the target of 100,000 cycles without failure, unlike the as-built samples, which failed prematurely. The fractography analysis identified surface porosity as the primary crack initiation site. The findings suggest that low-temperature stress-relieving treatment can enhance the fatigue performance of L-PBF AlSi10Mg components by reducing residual stresses and improving defect tolerance.
format Article
id doaj-art-fc55c5038a494ebd8ebbb95838c72752
institution Kabale University
issn 2076-3417
language English
publishDate 2024-12-01
publisher MDPI AG
record_format Article
series Applied Sciences
spelling doaj-art-fc55c5038a494ebd8ebbb95838c727522025-01-10T13:14:29ZengMDPI AGApplied Sciences2076-34172024-12-0115111210.3390/app15010112Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10MgMalcolm António0Rui Fernandes1Joel de Jesus2Luís Borrego3Ricardo Branco4José da Costa5José Ferreira6CEMMPRE, ARISE, Department of Mechanical Engineering, University of Coimbra, Rua Luís Reis Santos, 3030-788 Coimbra, PortugalCEMMPRE, ARISE, Department of Mechanical Engineering, University of Coimbra, Rua Luís Reis Santos, 3030-788 Coimbra, PortugalCEMMPRE, ARISE, Department of Mechanical Engineering, University of Coimbra, Rua Luís Reis Santos, 3030-788 Coimbra, PortugalCEMMPRE, ARISE, Department of Mechanical Engineering, University of Coimbra, Rua Luís Reis Santos, 3030-788 Coimbra, PortugalCEMMPRE, ARISE, Department of Mechanical Engineering, University of Coimbra, Rua Luís Reis Santos, 3030-788 Coimbra, PortugalCEMMPRE, ARISE, Department of Mechanical Engineering, University of Coimbra, Rua Luís Reis Santos, 3030-788 Coimbra, PortugalCEMMPRE, ARISE, Department of Mechanical Engineering, University of Coimbra, Rua Luís Reis Santos, 3030-788 Coimbra, PortugalThis study investigates the impact of low-temperature stress-relieving treatment on the fatigue life of AlSi10Mg components produced by Laser Powder Bed Fusion (L-PBF). The research focuses on a bicycle crank arm, comparing its performance in as-built and heat-treated conditions. The heat treatment involved stress-relieving at 250 °C for 2 h, followed by water quenching. The study found that the as-built condition exhibited a supersaturated Si cellular-dendritic microstructure, while the heat-treated condition showed coarsening of β-Mg<sub>2</sub>Si phases and Si precipitates. This morphological change led to a decrease in hardness and an increase in ductility. Fatigue tests demonstrated that the heat-treated crank arms achieved the target of 100,000 cycles without failure, unlike the as-built samples, which failed prematurely. The fractography analysis identified surface porosity as the primary crack initiation site. The findings suggest that low-temperature stress-relieving treatment can enhance the fatigue performance of L-PBF AlSi10Mg components by reducing residual stresses and improving defect tolerance.https://www.mdpi.com/2076-3417/15/1/112L-PBFheat treatmentfatiguealuminum alloylaser additive manufacturingstress relief
spellingShingle Malcolm António
Rui Fernandes
Joel de Jesus
Luís Borrego
Ricardo Branco
José da Costa
José Ferreira
Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10Mg
Applied Sciences
L-PBF
heat treatment
fatigue
aluminum alloy
laser additive manufacturing
stress relief
title Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10Mg
title_full Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10Mg
title_fullStr Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10Mg
title_full_unstemmed Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10Mg
title_short Influence of Low-Temperature Stress-Relieving Treatment in the Fatigue Life of Components Produced by Laser Powder Bed Fusion in AlSi10Mg
title_sort influence of low temperature stress relieving treatment in the fatigue life of components produced by laser powder bed fusion in alsi10mg
topic L-PBF
heat treatment
fatigue
aluminum alloy
laser additive manufacturing
stress relief
url https://www.mdpi.com/2076-3417/15/1/112
work_keys_str_mv AT malcolmantonio influenceoflowtemperaturestressrelievingtreatmentinthefatiguelifeofcomponentsproducedbylaserpowderbedfusioninalsi10mg
AT ruifernandes influenceoflowtemperaturestressrelievingtreatmentinthefatiguelifeofcomponentsproducedbylaserpowderbedfusioninalsi10mg
AT joeldejesus influenceoflowtemperaturestressrelievingtreatmentinthefatiguelifeofcomponentsproducedbylaserpowderbedfusioninalsi10mg
AT luisborrego influenceoflowtemperaturestressrelievingtreatmentinthefatiguelifeofcomponentsproducedbylaserpowderbedfusioninalsi10mg
AT ricardobranco influenceoflowtemperaturestressrelievingtreatmentinthefatiguelifeofcomponentsproducedbylaserpowderbedfusioninalsi10mg
AT josedacosta influenceoflowtemperaturestressrelievingtreatmentinthefatiguelifeofcomponentsproducedbylaserpowderbedfusioninalsi10mg
AT joseferreira influenceoflowtemperaturestressrelievingtreatmentinthefatiguelifeofcomponentsproducedbylaserpowderbedfusioninalsi10mg