Optimization of Vanadium Content for Achieving Higher Wear Resistance and Hardness in High Cr-V White Cast Irons for Ball Tube Mill Liner Application
The liner materials, being used, at present from high Cr cast iron grades in coal fired tube mills are less promising due to lower combination of abrasion wear resistance, hardness and impact toughness properties, thus giving life of only 25,000 to 35,000 hours. In this study, focus was given to dev...
Saved in:
| Main Authors: | Dhirendra Kumar, G. Jayaraman, M. Swamy, Pavan A. H. V., Antony Harison M. C., A. N. Sudhakar |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Gruppo Italiano Frattura
2019-06-01
|
| Series: | Fracture and Structural Integrity |
| Subjects: | |
| Online Access: | https://www.fracturae.com/index.php/fis/article/view/2275 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Optimization of Vanadium Content for Achieving Higher Wear Resistance and Hardness in High Cr-V White Cast Irons for Ball Tube Mill Liner Application
by: Dhirendra Kumar, et al.
Published: (2019-07-01) -
Microstructure Formation and Dry Reciprocating Sliding Wear Response of High-Entropy Hypereutectic White Cast Irons
by: Willian Martins Pasini, et al.
Published: (2024-12-01) -
Effect of Pressure on the Microstructure and Wear Performance of Cr-Mn-Mo Alloyed Steel Prepared by Squeeze Casting
by: Yuan Zhuang, et al.
Published: (2024-11-01) -
Microstructure, hardness, and wear resistance of high-carbon hypereutectic high chromium irons containing W for use as roller sleeves
by: Shuang Liu, et al.
Published: (2024-11-01) -
Application of cast parts in mechanical engineering
by: M. A. Sadokha, et al.
Published: (2022-05-01)