Laser Beam Welding of AA5052, AA5083, and AA6061 Aluminum Alloys
The present investigation was mainly concerned with characteristics of autogeneous laser butt welding of 2 mm thickness nonheat treatableAA5052-H12,AA5083-H12 and 2 mm, 3 mm thickness heat treatableAA6061-T6aluminum alloys. The effect of laser welding parameters, surface cleaning, filler wire additi...
Saved in:
Main Authors: | A. El-Batahgy, M. Kutsuna |
---|---|
Format: | Article |
Language: | English |
Published: |
Wiley
2009-01-01
|
Series: | Advances in Materials Science and Engineering |
Online Access: | http://dx.doi.org/10.1155/2009/974182 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Studying the effect of processing parameters on the microstructure, strength, hardness, and corrosion characteristics of friction stir dissimilar welded AA5083 and AA7075 aluminum alloys reinforced with Al-SiC matrix
by: Noha M. Abdeltawab, et al.
Published: (2025-01-01) -
Experimental investigation of hardness of FSW and TIG joints of Aluminium alloys of AA7075 and AA6061
by: Chetan Patil, et al.
Published: (2016-06-01) -
Optimization of Ultimate Tensile Strength with DOE Approach for Application FSW Process in the Aluminum alloys AA6061-T651 & AA7075 -T651
by: Mohammed Chaib, et al.
Published: (2021-06-01) -
Optimization of Process Parameters for Friction Stir Welding of Different Aluminum Alloys AA2618 to AA5086 by Taguchi Method
by: G. Sasikala, et al.
Published: (2022-01-01) -
Investigation of Using the IL-FSSW Technique to Weld AA5052-H112 Alloy with Copper: Experimental Study
by: Kareem Abbas Falih, et al.
Published: (2023-12-01)