CRYOGENIC RATCHETING OF PRESTRAINED AUSTENITIC STAINLESS STEEL S30408
Taking advantage of the EUM-25 K20 tension-torsion fatigue testing machine by CARE,the cryogenic uniaxial ratcheting tests were carried out for the S30408 specimens with and without weld,and with 0%,8%,and 12% pre-strains at110 K. It is shown that ratcheting behavior of specimens with and without we...
Saved in:
Main Authors: | LI LeiLei, GAO BingJun, DONG JunHua, CHEN Xu |
---|---|
Format: | Article |
Language: | zho |
Published: |
Editorial Office of Journal of Mechanical Strength
2020-01-01
|
Series: | Jixie qiangdu |
Subjects: | |
Online Access: | http://www.jxqd.net.cn/thesisDetails#10.16579/j.issn.1001.9669.2020.05.008 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
PRE-STRAIN EFFECT EVALUATION OF AUSTENITIC STAINLESS STEEL
by: LIU XiaoNing, et al.
Published: (2019-01-01) -
Ratcheting of 316L stainless steel thin wire under tension-torsion loading
by: Sichao Fu, et al.
Published: (2016-10-01) -
EFFECT OF HEATING MODE ON THE STRIP STRENGTH OF THE CRYOGENIC STORAGE TANK DURING VACUUMIZING
by: WANG Bin, et al.
Published: (2018-01-01) -
Evaluation of the ratcheting behavior of Cr-Mo steel used in CNG tank
by: Karim Aliakbari, et al.
Published: (2025-03-01) -
Capillary Skimming of Floating Microplastics via a Water‐Bridged Ratchet
by: Seohyun Cho, et al.
Published: (2025-01-01)