Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine Oil
In general, vegetable oils are chosen for oil heat treatment. Oil heat treatment with waste engine oil, which is quite limited in the literature, was used in this study. After the wood material was subjected to oil heat treatment with waste motor oil, several physical parameters such as oven-dry and...
Saved in:
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
University of Zagreb, Faculty of Forestry and Wood Technology
2024-01-01
|
Series: | Drvna Industrija |
Subjects: | |
Online Access: | https://hrcak.srce.hr/file/470691 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
_version_ | 1841561002610524160 |
---|---|
author | Caglar Altay Davut Çiftçi Hilmi Toker Ergün Baysal |
author_facet | Caglar Altay Davut Çiftçi Hilmi Toker Ergün Baysal |
author_sort | Caglar Altay |
collection | DOAJ |
description | In general, vegetable oils are chosen for oil heat treatment. Oil heat treatment with waste engine oil, which is quite limited in the literature, was used in this study. After the wood material was subjected to oil heat treatment with waste motor oil, several physical parameters such as oven-dry and air-dry density, water absorption (WA) levels, and mechanical properties such as compression strength parallel to the grain (CSPG) were examined. The color changes of waste engine oil heat treated (WEOHT) specimens were examined after three months of weathering. The results showed that when oven-dry and air-dry density of WEOHT specimens increased, WA levels decreased. The WEOHT specimens had greater CSPG values than the control group. WEOHT specimens and control group revealed negative ΔL*, Δa*, and Δb* values following weathering. The WEOHT specimens had smaller total colorchanges (ΔE*) than the control group after weathering. Our results showed that higher temperature and durations resulted in lower WA, and higher air-dry density and total color changes of WEOHT specimens. |
format | Article |
id | doaj-art-ddc1a84cd68e494191b83e2f87eeac6b |
institution | Kabale University |
issn | 0012-6772 1847-1153 |
language | English |
publishDate | 2024-01-01 |
publisher | University of Zagreb, Faculty of Forestry and Wood Technology |
record_format | Article |
series | Drvna Industrija |
spelling | doaj-art-ddc1a84cd68e494191b83e2f87eeac6b2025-01-03T09:03:08ZengUniversity of Zagreb, Faculty of Forestry and Wood TechnologyDrvna Industrija0012-67721847-11532024-01-0175446947810.5552/drvind.2024.0203Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine OilCaglar Altay0Davut Çiftçi1Hilmi Toker2Ergün Baysal3aydin adnan menderes university, Aydin, TurkeyMuğla Sıtkı Koçman Üniversitesi, Muğla, TurkeyMuğla Sıtkı Koçman University, MUĞLA, TurkeyMUĞLA SITKI KOÇMAN UNİVERSİTY, Muğla, TurkeyIn general, vegetable oils are chosen for oil heat treatment. Oil heat treatment with waste engine oil, which is quite limited in the literature, was used in this study. After the wood material was subjected to oil heat treatment with waste motor oil, several physical parameters such as oven-dry and air-dry density, water absorption (WA) levels, and mechanical properties such as compression strength parallel to the grain (CSPG) were examined. The color changes of waste engine oil heat treated (WEOHT) specimens were examined after three months of weathering. The results showed that when oven-dry and air-dry density of WEOHT specimens increased, WA levels decreased. The WEOHT specimens had greater CSPG values than the control group. WEOHT specimens and control group revealed negative ΔL*, Δa*, and Δb* values following weathering. The WEOHT specimens had smaller total colorchanges (ΔE*) than the control group after weathering. Our results showed that higher temperature and durations resulted in lower WA, and higher air-dry density and total color changes of WEOHT specimens.https://hrcak.srce.hr/file/470691oil heat treatmentoriental beechphysical propertiesmechanical propertiescolorwaste engine oil |
spellingShingle | Caglar Altay Davut Çiftçi Hilmi Toker Ergün Baysal Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine Oil Drvna Industrija oil heat treatment oriental beech physical properties mechanical properties color waste engine oil |
title | Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine Oil |
title_full | Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine Oil |
title_fullStr | Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine Oil |
title_full_unstemmed | Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine Oil |
title_short | Physical, Mechanical and Weathering Characteristics of Oriental beech Heat Treated with Waste Engine Oil |
title_sort | physical mechanical and weathering characteristics of oriental beech heat treated with waste engine oil |
topic | oil heat treatment oriental beech physical properties mechanical properties color waste engine oil |
url | https://hrcak.srce.hr/file/470691 |
work_keys_str_mv | AT caglaraltay physicalmechanicalandweatheringcharacteristicsoforientalbeechheattreatedwithwasteengineoil AT davutciftci physicalmechanicalandweatheringcharacteristicsoforientalbeechheattreatedwithwasteengineoil AT hilmitoker physicalmechanicalandweatheringcharacteristicsoforientalbeechheattreatedwithwasteengineoil AT ergunbaysal physicalmechanicalandweatheringcharacteristicsoforientalbeechheattreatedwithwasteengineoil |