Parameters Controlling the Oxide Reduction during Sintering of Chromium Prealloyed Steel
Temperature intervals of oxide reduction processes during sintering of the Fe-3%Cr-0.5%Mo prealloyed powder using continuous monitoring of processing-exhaust gas composition (CO, CO2, and H2O) were identified and interpreted in relation to density (6.5–7.4 g/cm3), sintering temperature (1120 and 120...
Saved in:
| Main Authors: | Monika Hrubovčáková, Eva Dudrová, Eduard Hryha, Margita Kabátová, Jarmila Harvanová |
|---|---|
| Format: | Article |
| Language: | English |
| Published: |
Wiley
2013-01-01
|
| Series: | Advances in Materials Science and Engineering |
| Online Access: | http://dx.doi.org/10.1155/2013/789373 |
| Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Experimental Study on Disposal of Chromium-containing Sludge by Sintering
by: Shizhe SONG, et al.
Published: (2024-12-01) -
Influence of iron ore concentrate on the characteristics of sintering and reduction of sinter
by: Guo H., et al.
Published: (2020-01-01) -
On the formation of oxide inclusions in the high nitrogen chromium-manganese steel produced by the Wire and Arc Additive Manufacturing
by: Xiaoyong Zhang, et al.
Published: (2024-11-01) -
Reduction of Chromium and Manganese Heavy Metal Concentration in Leachate by Electrocoagulation
by: Tricia Danica C. Calma, et al.
Published: (2024-12-01) -
Correlation of Process Parameters with Mechanical Properties of Laser Sintered PA12 Parts
by: Eva C. Hofland, et al.
Published: (2017-01-01)