Statistical Peculiar Features of Surface Cracking on Flat Clay Samples of Plastic Moulding when Heated by Heat Flow
Results of 240 time determinations pertaining to investigation of surface cracking initiation on flat samples of moulding mass (80% of the Lukoml clay + 20% of granite screenings) of various thickness (1 ...4 cm) while being heated with intensive heat flow (~ 1 W/cm2) are given and analyzed in the p...
Saved in:
Main Author: | I. K. Ivanovsky |
---|---|
Format: | Article |
Language: | Russian |
Published: |
Belarusian National Technical University
2003-08-01
|
Series: | Известия высших учебных заведений и энергетических объединенний СНГ: Энергетика |
Online Access: | https://energy.bntu.by/jour/article/view/1271 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
SOME PECULIAR FEATURES IN SHRINKAGE OF CLAY MASS DURING DRYING PROCESS
by: I. K. Ivanovsky, et al.
Published: (2005-12-01) -
Heat Transport and Water Permeability during Cracking of the Landfill Compacted Clay Cover
by: Haijun Lu, et al.
Published: (2015-01-01) -
Combined lock-in thermography and heat flow measurements for analysing heat dissipation during fatigue crack propagation
by: J. Baer, et al.
Published: (2015-09-01) -
Combined lock-in thermography and heat flow measurements for analysing heat dissipation during fatigue crack propagation
by: J. Bär, et al.
Published: (2015-10-01) -
Investigation on the Achievable Flow Length in Injection Moulding of Polymeric Materials with Dynamic Mould Tempering
by: Steve Meister, et al.
Published: (2013-01-01)