Removal of iron and manganese from acidic aqueous solution by pyrite and pyrite-calcium sulfite
Abstract Pyrite and calcium sulfite were used to remove iron and manganese from an acidic aqueous solution. The concentration of Fe was decreased to be smaller than 0.05 g/L in 60 min when pyrite and air were added into the acidic aqueous solution, but the concentration of Mn in the solution remaine...
Saved in:
Main Authors: | Xu Zhang, Yajing Wang, Gesang Nima, Ziqian Wang, Caifeng Huang |
---|---|
Format: | Article |
Language: | English |
Published: |
Nature Portfolio
2025-02-01
|
Series: | Scientific Reports |
Subjects: | |
Online Access: | https://doi.org/10.1038/s41598-025-88448-9 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
The effect of iron and oxidizing flux addition on the fire assay of low grade pyritic refractory gold ores
by: Turan A., et al.
Published: (2011-01-01) -
Preparation and recovery of iron carbide from pyrite cinder using carburization-magnetic separation technology
by: Chen D., et al.
Published: (2018-01-01) -
Separation of iron-nickel alloy nugget from limonitic laterite ore using self-reduction
by: Ju P., et al.
Published: (2018-01-01) -
Viscosity and structure evolution of the SiO2-MgO-FeO-CaO-Al2O3 slag in ferronickel smelting process from laterite
by: Lv X.M., et al.
Published: (2017-01-01) -
Study of initial stage of mechanochemical transformation in pyrite
by: Paneva D., et al.
Published: (2007-01-01)