STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEEL

Shot peening process is widely used in the manufacturing process of gears and other basic components, and its own limitations limit the enhancement of the surface integrity of the workpiece. In order to further improve the surface integrity of the workplece, A combination of numerical simulation and...

Full description

Saved in:
Bibliographic Details
Main Authors: WANG Zhen, SUN Hao, CUI YiLong, LI LinYan, WANG Tao, HAN JiaoBao
Format: Article
Language:zho
Published: Editorial Office of Journal of Mechanical Strength 2024-01-01
Series:Jixie qiangdu
Subjects:
Online Access:http://www.jxqd.net.cn/thesisDetails?columnId=59755117&Fpath=home&index=0
Tags: Add Tag
No Tags, Be the first to tag this record!
_version_ 1841534142744887296
author WANG Zhen
SUN Hao
CUI YiLong
LI LinYan
WANG Tao
HAN JiaoBao
author_facet WANG Zhen
SUN Hao
CUI YiLong
LI LinYan
WANG Tao
HAN JiaoBao
author_sort WANG Zhen
collection DOAJ
description Shot peening process is widely used in the manufacturing process of gears and other basic components, and its own limitations limit the enhancement of the surface integrity of the workpiece. In order to further improve the surface integrity of the workplece, A combination of numerical simulation and experimental methods was utilized to study the effect of two surface composite strengthening processes, such as double shot peening and shot peening-ultrasonic rolling, on the surface integrity of 18CrNiMo7-6 carburization gear steel samples, and mainly analyzed the effect of the two composite strengthening processes on the improvement of surface integrity of the shot peened samples. The results show that the maximum value of the residual compressive stress of the double shot peening sample is 1 359.56 MPa, locates at the depth of 0.08 mm, and the maximum value of the residual compressive stress of the shot peening-ultrasonic rolling peening sample is 1 329.05 MPa, locates at the depth of 0.25 mm. Compare with the single shot peening sample, the surface roughness of the double shot peening sample and the shot peening-ultrasonic rolling sample is 29.42% and 29.42% lower than that of the single shot peening sample. Compare with the single shot peening samples, the surface roughness of the double shot peening samples and shot peening-ultrasonic tumbling peening samples decreases by 29.42% and 62.76%, respectively, the surface microhardness increases by 8.70% and 17.60%, and the standard deviation of the surface node compressive residual stress value decreases by 23.36% and 89.50%. The shot peening-ultrasonic rolling process is more effective in enhancing the surface hardness, thickness of the residual stress layer and uniformity of the residual compressive stress, as well as reducing the surface roughness of the specimens, and can effectively improve the surface integrity of the shot peened samples.
format Article
id doaj-art-0df9efebbc8e4cb9ae3cd24e0572b6c7
institution Kabale University
issn 1001-9669
language zho
publishDate 2024-01-01
publisher Editorial Office of Journal of Mechanical Strength
record_format Article
series Jixie qiangdu
spelling doaj-art-0df9efebbc8e4cb9ae3cd24e0572b6c72025-01-15T02:44:52ZzhoEditorial Office of Journal of Mechanical StrengthJixie qiangdu1001-96692024-01-0111259755117STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEELWANG ZhenSUN HaoCUI YiLongLI LinYanWANG TaoHAN JiaoBaoShot peening process is widely used in the manufacturing process of gears and other basic components, and its own limitations limit the enhancement of the surface integrity of the workpiece. In order to further improve the surface integrity of the workplece, A combination of numerical simulation and experimental methods was utilized to study the effect of two surface composite strengthening processes, such as double shot peening and shot peening-ultrasonic rolling, on the surface integrity of 18CrNiMo7-6 carburization gear steel samples, and mainly analyzed the effect of the two composite strengthening processes on the improvement of surface integrity of the shot peened samples. The results show that the maximum value of the residual compressive stress of the double shot peening sample is 1 359.56 MPa, locates at the depth of 0.08 mm, and the maximum value of the residual compressive stress of the shot peening-ultrasonic rolling peening sample is 1 329.05 MPa, locates at the depth of 0.25 mm. Compare with the single shot peening sample, the surface roughness of the double shot peening sample and the shot peening-ultrasonic rolling sample is 29.42% and 29.42% lower than that of the single shot peening sample. Compare with the single shot peening samples, the surface roughness of the double shot peening samples and shot peening-ultrasonic tumbling peening samples decreases by 29.42% and 62.76%, respectively, the surface microhardness increases by 8.70% and 17.60%, and the standard deviation of the surface node compressive residual stress value decreases by 23.36% and 89.50%. The shot peening-ultrasonic rolling process is more effective in enhancing the surface hardness, thickness of the residual stress layer and uniformity of the residual compressive stress, as well as reducing the surface roughness of the specimens, and can effectively improve the surface integrity of the shot peened samples.http://www.jxqd.net.cn/thesisDetails?columnId=59755117&Fpath=home&index=018CrNiMo7⁃6 steelShot peeningUltrasonic rollingSurface integrity
spellingShingle WANG Zhen
SUN Hao
CUI YiLong
LI LinYan
WANG Tao
HAN JiaoBao
STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEEL
Jixie qiangdu
18CrNiMo7⁃6 steel
Shot peening
Ultrasonic rolling
Surface integrity
title STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEEL
title_full STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEEL
title_fullStr STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEEL
title_full_unstemmed STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEEL
title_short STUDY ON THE EFFECT OF SURFACE COMPOSITE STRENGTHENING ON THE SURFACE INTEGRITY OF 18CrNiMo7⁃6 CARBURIZED GEAR STEEL
title_sort study on the effect of surface composite strengthening on the surface integrity of 18crnimo7⁃6 carburized gear steel
topic 18CrNiMo7⁃6 steel
Shot peening
Ultrasonic rolling
Surface integrity
url http://www.jxqd.net.cn/thesisDetails?columnId=59755117&Fpath=home&index=0
work_keys_str_mv AT wangzhen studyontheeffectofsurfacecompositestrengtheningonthesurfaceintegrityof18crnimo76carburizedgearsteel
AT sunhao studyontheeffectofsurfacecompositestrengtheningonthesurfaceintegrityof18crnimo76carburizedgearsteel
AT cuiyilong studyontheeffectofsurfacecompositestrengtheningonthesurfaceintegrityof18crnimo76carburizedgearsteel
AT lilinyan studyontheeffectofsurfacecompositestrengtheningonthesurfaceintegrityof18crnimo76carburizedgearsteel
AT wangtao studyontheeffectofsurfacecompositestrengtheningonthesurfaceintegrityof18crnimo76carburizedgearsteel
AT hanjiaobao studyontheeffectofsurfacecompositestrengtheningonthesurfaceintegrityof18crnimo76carburizedgearsteel